Because the chemical states of the elements in SrTiO3 thin film on Si are reduced by argon ion beam bombardment, it was impossible to sputter depth profile the chemical states of SrTiO3 thin film by argon ion beams, In this paper, it is reported that the undistorted chemical states of Ti and Si at the SrTiO3/Si interface can be determined with oxygen ion beams at the appropriate 70 degrees angle of incidence, with which either metallic Ti is not oxidized or Ti in SrTiO3 is not reduced, Under the sputter depth profiling conditions, the chemical state of Ti at the SrTiO3/Si interface could be successfully characterized and the effects of post-annealing at high temperature on the chemical state of Ti were studied, A significant number of Ti atoms in the metallic state were observed at the SrTiO3/Si interface without any post-annealing but all of them were oxidized to the Ti4+ chemical state after 2 h post-annealing at the temperatures above 600 degrees C under oxygen flow, The dielectric properties of SrTiO3 thin films on Si were well correlated to the oxidation state of Ti and the broadening of the interface SiO2 layer induced by post-annealing at high temperature.
Publisher
JOHN WILEY & SONS LTD
Issue Date
1995-12
Language
English
Article Type
Article
Citation

SURFACE INTERFACE ANALYSIS, v.23, no.13, pp.851 - 857

ISSN
0142-2421
DOI
10.1002/sia.740231302
URI
http://hdl.handle.net/10203/71874
Appears in Collection
MS-Journal Papers(저널논문)
Files in This Item
There are no files associated with this item.
This item is cited by other documents in WoS
⊙ Detail Information in WoSⓡ Click to see webofscience_button
⊙ Cited 16 items in WoS Click to see citing articles in records_button

qr_code

  • mendeley

    citeulike


rss_1.0 rss_2.0 atom_1.0