Enhanced nucleation of diamond on polycrystalline Ni by d.c. glow discharge in hot filament CVD

Cited 7 time in webofscience Cited 7 time in scopus
  • Hit : 296
  • Download : 0
If a negative glow discharge is produced around a cathode wire above a polycrystalline Ni substrate, the diamond nucleation rate is greatly enhanced in the hot filament chemical deposition process. The diamond deposition depends on the surface orientation of the Ni grains, and occurs preferentially on faceted surfaces with hill-and-valley structures. The deposited diamond particles show a tendency to orient in one direction. (C) 2000 Elsevier Science S.A. All rights reserved.
Publisher
ELSEVIER SCIENCE SA
Issue Date
2000-08
Language
English
Article Type
Article
Keywords

CHEMICAL-VAPOR-DEPOSITION; ORIENTATIONAL PHASE-DIAGRAM; SILICON; NICKEL; FILMS; GROWTH; HETEROEPITAXY; INTERFACES; MECHANISM; SUBSTRATE

Citation

DIAMOND AND RELATED MATERIALS, v.9, no.8, pp.1475 - 1479

ISSN
0925-9635
DOI
10.1016/S0925-9635(00)00272-7
URI
http://hdl.handle.net/10203/70863
Appears in Collection
Files in This Item
There are no files associated with this item.
This item is cited by other documents in WoS
⊙ Detail Information in WoSⓡ Click to see webofscience_button
⊙ Cited 7 items in WoS Click to see citing articles in records_button

qr_code

  • mendeley

    citeulike


rss_1.0 rss_2.0 atom_1.0