Tracking and Erosion Resistance of High Temperature Vulcanizing ATH-free Silicone Rubber

Cited 50 time in webofscience Cited 0 time in scopus
  • Hit : 225
  • Download : 0
DC FieldValueLanguage
dc.contributor.authorSchmidt, Lars E.ko
dc.contributor.authorKornmann, Xavierko
dc.contributor.authorKrivda, Andrejko
dc.contributor.authorHillborg, Henrikko
dc.date.accessioned2017-10-23T02:40:10Z-
dc.date.available2017-10-23T02:40:10Z-
dc.date.created2017-10-17-
dc.date.created2017-10-17-
dc.date.issued2010-04-
dc.identifier.citationIEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, v.17, no.2, pp.533 - 540-
dc.identifier.issn1070-9878-
dc.identifier.urihttp://hdl.handle.net/10203/226662-
dc.description.abstractTraditionally aluminum trihydrate (ATH) is added to high-temperature vulcanized (HTV) silicone rubber for outdoor insulation applications to improve flame retardancy and the electrical tracking and erosion performance. In this work, the flammability of ATH-free HTV silicone rubber formulations were evaluated by the UL94 vertical burning test. The most promising candidates, as well as reference formulations filled with silica or silica/ATH only, were then evaluated by the inclined plane tracking and erosion test at 4.5 kV. The best result was obtained by silicone rubber containing 100 phr silica and 15 phr melamine cyanurate. It was suggested that this was a result of the arc quenching ability of the melamine hence extinguishing the electrical arc. If the filler level was too high, resulting in poor dispersion, the resistance to tracking and erosion was significantly reduced. Thus formulating a HTV silicone rubber with good tracking and erosion resistance is a balance between having a high enough filler content, while still maintaining a good dispersion of the particles in the polymer matrix, as well as good bonding between the particles and the matrix.-
dc.languageEnglish-
dc.publisherIEEE-INST ELECTRICAL ELECTRONICS ENGINEERS INC-
dc.subjectDRY-BAND DISCHARGES-
dc.subjectOUTDOOR INSULATION-
dc.subjectPOLYDIMETHYLSILOXANE-
dc.titleTracking and Erosion Resistance of High Temperature Vulcanizing ATH-free Silicone Rubber-
dc.typeArticle-
dc.identifier.wosid000282023500026-
dc.identifier.scopusid2-s2.0-77951521846-
dc.type.rimsART-
dc.citation.volume17-
dc.citation.issue2-
dc.citation.beginningpage533-
dc.citation.endingpage540-
dc.citation.publicationnameIEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION-
dc.identifier.doi10.1109/TDEI.2010.5448109-
dc.contributor.localauthorSchmidt, Lars E.-
dc.contributor.nonIdAuthorKornmann, Xavier-
dc.contributor.nonIdAuthorKrivda, Andrej-
dc.contributor.nonIdAuthorHillborg, Henrik-
dc.description.isOpenAccessN-
dc.type.journalArticleArticle-
dc.subject.keywordAuthorSilicone rubber-
dc.subject.keywordAuthortracking-
dc.subject.keywordAuthorinsulation-
dc.subject.keywordPlusDRY-BAND DISCHARGES-
dc.subject.keywordPlusOUTDOOR INSULATION-
dc.subject.keywordPlusPOLYDIMETHYLSILOXANE-
Appears in Collection
RIMS Journal Papers
Files in This Item
There are no files associated with this item.
This item is cited by other documents in WoS
⊙ Detail Information in WoSⓡ Click to see webofscience_button
⊙ Cited 50 items in WoS Click to see citing articles in records_button

qr_code

  • mendeley

    citeulike


rss_1.0 rss_2.0 atom_1.0