High mobility polycrystalline indium oxide thin-film transistors by means of plasma-enhanced atomic layer deposition

Cited 89 time in webofscience Cited 0 time in scopus
  • Hit : 331
  • Download : 0
DC FieldValueLanguage
dc.contributor.authorYeom, Hye-Inko
dc.contributor.authorKo, Jong Beomko
dc.contributor.authorMun, Geumbiko
dc.contributor.authorPark, Sang-Hee Koko
dc.date.accessioned2016-09-07T01:45:56Z-
dc.date.available2016-09-07T01:45:56Z-
dc.date.created2016-08-16-
dc.date.created2016-08-16-
dc.date.created2016-08-16-
dc.date.issued2016-06-
dc.identifier.citationJOURNAL OF MATERIALS CHEMISTRY C, v.4, no.28, pp.6873 - 6880-
dc.identifier.issn2050-7526-
dc.identifier.urihttp://hdl.handle.net/10203/212590-
dc.description.abstractIndium oxide thin films are deposited via plasma-enhanced atomic layer deposition (PEALD) to exploit their potential as a semiconductor in high mobility thin-film transistors (TFTs), which are suitable for fast driving applications such as high resolution displays. The films are successfully grown by the reaction between an Et2InN(SiMe3)(2) liquid precursor and oxygen plasma at temperatures ranging from 100 degrees C to 250 degrees C giving a saturated growth rate value of similar to 1.45 angstrom per cycle at the ALD window with precisely controlled thickness and uniformity. The plasma reaction enhances the film growth rate and changes the electrical properties of the films. Depending on the substrate temperatures, each film has a different chemical composition, thereby showing different electrical characteristics. Indium oxide films grown by PEALD show a lower carrier density of similar to 4 x 10(19) cm(-3) than those prepared by thermal ALD due to the reactive oxygen plasma source in the former. Offering the precise control of thickness and high quality of indium oxide grown by PEALD, and with a proper post thermal-annealing and passivation process, the possibility of exploiting the potential of semiconductor characteristics of indium oxide is verified from bottom-gate coplanar structured TFTs, which exhibit a high mobility as high as 39.2 cm(2) V-1 s(-1), a turn-on voltage value of -1.18 V, and a sub-threshold voltage of 0.27 V dec(-1) in a linear region. On the basis of this outstanding performance, the PEALD-InOx TFTs developed in this study would be suitable for diverse microelectronic devices-
dc.languageEnglish-
dc.publisherRoyal Society of Chemistry-
dc.titleHigh mobility polycrystalline indium oxide thin-film transistors by means of plasma-enhanced atomic layer deposition-
dc.typeArticle-
dc.identifier.wosid000379871900023-
dc.identifier.scopusid2-s2.0-84978952291-
dc.type.rimsART-
dc.citation.volume4-
dc.citation.issue28-
dc.citation.beginningpage6873-
dc.citation.endingpage6880-
dc.citation.publicationnameJOURNAL OF MATERIALS CHEMISTRY C-
dc.identifier.doi10.1039/c6tc00580b-
dc.contributor.localauthorPark, Sang-Hee Ko-
dc.contributor.nonIdAuthorMun, Geumbi-
dc.type.journalArticleArticle-
dc.subject.keywordPlusELECTRICAL-PROPERTIES-
dc.subject.keywordPlusIN2O3-
dc.subject.keywordPlusTRANSPARENT-
dc.subject.keywordPlusPERFORMANCE-
dc.subject.keywordPlusGROWTH-
dc.subject.keywordPlusFABRICATION-
dc.subject.keywordPlusVOLTAGE-
Appears in Collection
MS-Journal Papers(저널논문)
Files in This Item
There are no files associated with this item.
This item is cited by other documents in WoS
⊙ Detail Information in WoSⓡ Click to see webofscience_button
⊙ Cited 89 items in WoS Click to see citing articles in records_button

qr_code

  • mendeley

    citeulike


rss_1.0 rss_2.0 atom_1.0