Showing results 1 to 3 of 3
Combinatorial studies of mechanical properties of Ti-Al thin films using nanoindentation Han, Seung Min J.; Shah, R; Banerjee, R; Viswanathan, GB; Clemens, BM; Nix, WD, ACTA MATERIALIA, v.53, no.7, pp.2059 - 2067, 2005-04 |
Determining hardness of thin films in elastically mismatched film-on-substrate systems using nanoindentation Han, Seung Min J.; Saha, R; Nix, WD, ACTA MATERIALIA, v.54, no.6, pp.1571 - 1581, 2006-04 |
Electronic-Mechanical Coupling in Graphene from in situ Nanoindentation Experiments and Multiscale Atomistic Simulations Huang, Mingyuan; Pascal, Tod A.; Kim, Hyungjun; Goddard, William A., III; Greer, Julia R., NANO LETTERS, v.11, no.3, pp.1241 - 1246, 2011-03 |