Showing results 1 to 1 of 1
Oxidation behaviors of wrought nickel-based superalloys in various high temperature environments Jang, Chang-Heui; Kim, Dae-Jong; Kim, Dong-Hoon; Sah, In-Jin; Ryu, Woo-Seog; Yoo, Young-sung, TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, v.21, no.7, pp.1524 - 1531, 2011-07 |