Microstructure evolution of a Ni-Cr-W superalloy during long-term aging at high temperatures

Lee, Ho Jung; Kim, Hyunmyung; Kim, Donghoon; Jang, Changheui, MATERIALS CHARACTERIZATION, v.106, pp.283 - 291, 2015-08