Showing results 1 to 2 of 2
Effects of PbO on the repassivation kinetics of alloy 690 Ahn, S; Rao, VS; Kwon, Hyuk-Sang; Kim, U, CORROSION SCIENCE, v.48, no.5, pp.1137 - 1153, 2006-05 |
붕소와 탄소가 단결정용 니켈기 초내열합금의 결함수용성에 미치는 효과 = Effect of boron and carbon on the defect tolerability of a nickel base single crystal superalloylink 김두현; Kim, Doo-Hyun; et al, 한국과학기술원, 2003 |