The effect of atmosphere control on the sintering behaviour of TiB2-20 wt % Ni ceramics was investigated. Sintering was performed at 1700 degrees C for 1 h with commercial TiB2 powders produced by the carbothermic reaction. Under a fixed single atmosphere such as vacuum or Ar, densification was limited and large pores remained. However, a sintered density above 99% of theoretical could be achieved by a two-step sintering procedure in which the atmosphere was changed from vacuum to Ar at 1600 degrees C during the heat-up with subsequent isothermal sintering being performed at 1700 degrees C for 1 h. Qualitative considerations about these phenomena are discussed.
Publisher
Kluwer Academic Publishers
Issue Date
1996
Language
English
Article Type
Article
Keywords

TITANIUM DIBORIDE; W-NI; DENSIFICATION; ATMOSPHERE; CERAMICS; GAS

Citation

JOURNAL OF MATERIALS SCIENCE, v.31, no.21, pp.5805 - 5809

ISSN
0022-2461
URI
http://hdl.handle.net/10203/74415
Appears in Collection
MS-Journal Papers(저널논문)
Files in This Item
There are no files associated with this item.
This item is cited by other documents in WoS
⊙ Detail Information in WoSⓡ Click to see webofscience_button
⊙ Cited 15 items in WoS Click to see citing articles in records_button

qr_code

  • mendeley

    citeulike


rss_1.0 rss_2.0 atom_1.0