dc.description | 학위논문(석사) - 한국과학기술원 : 재료공학과, 1986.2, [ [iii], 44 p. ] | - |
dc.language | kor | - |
dc.publisher | 한국과학기술원 | - |
dc.subject | Hydrogen storage capacity. | - |
dc.title | $LaNi_5$ 및 $LaNi_{4.7}Al_{0.3}$ 의 temperature-induced-cycling 에 따른 intrinsic degradation 현상에 대한 연구 | - |
dc.title.alternative | A study on the intrinsic degradation phenomena of $LaNi_5$ and $LaNi_{4.7}Al_{0.3}$ during temperature-induced-cycling | - |
dc.type | Thesis(Master) | - |
dc.identifier.CNRN | 65410/325007 | - |
dc.description.department | 한국과학기술원 : 재료공학과, | - |
dc.identifier.uid | 000841123 | - |
dc.contributor.localauthor | 이재영 | - |
dc.contributor.localauthor | Lee, Jai-Young | - |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.