Browse by Title 

Showing results 150521 to 150540 of 279418

150521
Oxidation behavior of alumina-forming duplex stainless steels in high temperature steam environments = 고온 수증기 환경에서 알루미나 형성 듀플렉스 스테인리스강의 산화 거동link

Kim, Chaewon; Jang, Changheui; et al, 한국과학기술원, 2019

150522
Oxidation behavior of Fe-20Cr-25Ni-Nb austenitic stainless steel in high-temperature environment with small amount of water vapor

Chen, Hongsheng; Wang, Haibo; Sun, Qingzhu; Long, Chongsheng; Wei, Tianguo; Kim, Sung Hwan; Chen, Junjie; et al, CORROSION SCIENCE, v.145, pp.90 - 99, 2018-12

150523
Oxidation behavior of high-strength FeCrAl alloys in a high-temperature supercritical carbon dioxide environment

Chen, Hongsheng; Kim, Sung Hwan; Long, Chongsheng; Kim, Chaewon; Jang, Changheui, PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, v.28, no.6, pp.731 - 739, 2018-12

150524
Oxidation behavior of sintered tubular silicon carbide in pure steam I: Experiments

Lee, Youho; McKrell, Thomas J.; Montecot, Aline; Pantano, Michael; Song, Yann; Kazimi, Mujid S., CERAMICS INTERNATIONAL, v.42, no.1, pp.1916 - 1925, 2016-01

150525
Oxidation behavior of sintered tubular silicon carbide in pure steam II: Weight-loss correlation developments

Lee, Youho; McKrell, Thomas J.; Kazimi, Mujid S., CERAMICS INTERNATIONAL, v.42, no.4, pp.4679 - 4689, 2016-03

150526
Oxidation behavior of the directed energy deposited 316L stainless steel in supercritical carbon dioxide environment: Effect of post-manufacturing heat treatment

Chen, Junjie; Lee, Hyeon Bae; Jeong, Chaewon; Xiao, Qian; Jang, Kyungnam; An, Taejeong; Jang, Changheui, ADDITIVE MANUFACTURING, v.81, 2024-02

150527
Oxidation behavior of ZrB2-xSiC composites at 1500 degrees C under different oxygen partial pressures

Seong, Young Hoon; Kim, Do Kyung, CERAMICS INTERNATIONAL, v.40, no.9, pp.15303 - 15311, 2014-11

150528
Oxidation Behaviors of Nickel-Base Superalloys in High Temperature Steam Environments

김동훈; 장창희; 구자현; 김대종; 유영성, Transactions of the Korean Society of Pressure Vessels and Piping, v.7, pp.26 - 33, 2011-02

150529
Oxidation behaviors of wrought Nickel-base superalloys in high temperature nuclear environments

Jang, Changheui, IUMRS 11th International Conference in Asia, 2010-09-28

150530
Oxidation behaviors of wrought nickel-based superalloys in various high temperature environments

Jang, Chang-Heui; Kim, Dae-Jong; Kim, Dong-Hoon; Sah, In-Jin; Ryu, Woo-Seog; Yoo, Young-sung, TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, v.21, no.7, pp.1524 - 1531, 2011-07

150531
Oxidation behaviour of an Alloy 617 in very high-temperature air and helium environments

Jang, Changheui; Lee, Daejin; Kim, Daejong, INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, v.85, no.6, pp.368 - 377, 2008-06

150532
Oxidation Characteristics and Oxide Layer Evolution of Alloy 617 and Haynes 230 at 900 A degrees C and 1100 A degrees C

Kim, Daejong; Jang, Changheui; Ryu, Woo Seog, OXIDATION OF METALS, v.71, no.5-6, pp.271 - 293, 2009-06

150533
Oxidation characteristics of airborne carbon nanoparticles by NO2

Choo, Jung-Bum; Jung, Jae-Hee; Kim, Woo-Jin; Oh, Hyun-Cheol; Kim, Jin-Ho; Kim, Hak-Joon; Kim, Yong-Jin; et al, SCIENCE OF THE TOTAL ENVIRONMENT, v.405, no.1-3, pp.396 - 401, 2008-11

150534
Oxidation characteristics of Nickel-base superalloys at high temperature in air and helium atmospheres

Lee, D.; Kim, D.; Jang, Changheui, Societe Francaise d'Energie Nucleaire - International Congress on Advances in Nuclear Power Plants - ICAPP 2007, The Nuclear Renaissance at Work, pp.2360 - 2365, 2007-05-13

150535
Oxidation characteristics of the electron beam surface-treated Alloy 617 in high temperature helium environments

Lee, Ho Jung; Sah, Injin; Kim, Dong-Hoon; Kim, Hyunmyung; Jang, Chang-Heui, JOURNAL OF NUCLEAR MATERIALS, v.456, pp.220 - 227, 2015-01

150536
Oxidation effect on densification of CuInS2 absorber layer by paste coating

Lee S.-Y.; Kim K.-H.; Park B.-O., THIN SOLID FILMS, v.516, no.15, pp.4709 - 4712, 2008

150537
Oxidation effect on the loss characteristics of CPWs implemented on low resistivity substrate with thick Oxidized Porous Silicon(OPS) layer

Kwon, Young Se, EUMC, 2003

150538
Oxidation effects on the fracture toughness of the nuclear graphite at high temperature = 고온에서 원자력급 흑연의 파괴인성에 대한 산화 효과 연구link

Kim, Byung-jun; 김병준; et al, 한국과학기술원, 2008

150539
Oxidation Effects on the Strength and Fracture Toughness of the Selected Nuclear Graphite Grades at 600 ¡ÆC

Kim, Byung Jun; Kim, Daejong; Jang, Changheui; Chi, Se-Hwan, CARBON 2007, 2007-07-18

150540
Oxidation mechanism and kinetics of nuclear-grade FeCrAl alloys in the temperature range of 500-1500 degrees C in steam

Kim, Chaewon; Tang, Chongchong; Grosse, Mirco; Maeng, Yunhwan; Jang, Changheui; Steinbrueck, Martin, JOURNAL OF NUCLEAR MATERIALS, v.564, 2022-06